    descrizione del prodotto

    BÖHLER A204 is a stainless austenitic Cr-Ni-Mo steel with low carbon content. Resistant to intergranular corrosion up to 750°F (400°C). Heat treatment after welding not required.
    Good resistance to reducing acids, such as diluted sulfuric and hydrochloric acid, and to localized corrosion attack in media containing chlorine ions. Required surface finish pickled or polished. Very good cold formability, highly polishable.

    Use for watch industry, apparatus in the chemical, paper, cellulose, textile and pharmaceutical industries. Nuclear technology: Equipment subject to increased corrosion stress, also by media containing Cl, e.g. steam generator and superheater tubes in pressurized water reactors, condenser tubes, tube plates, fittings.

    proprietà

    • Good polishability due to a high degree of cleanliness 
    • High corrosion resistance (high content of Cr, Mo and N)
    • Homogeneous and stable autensic microstructure
    • Compliant to current standards, RoHS, …
    • Very low level concerning nickel release

     

    Steelmaking Process:  Airmelt

    Chemical Analysis:       lean + low S, Ni, Mo, less Ti, Nb, V

    Ferrite Content:             minor, max. 0,5%

    Cleanliness:                   good, DIN K3 max. 10

    Grain Size:                     6 and finer

    Polishabaility:               good

    Corrosion Resistance: good

    analisi chimica

    analisi chimica (media %)
    max. 0.030 max. 1.00 max. 2.00 max. 0.045 max. 0.030 17.0 to 19.0 2.50 to 3.00 12.5 to 15.0 max. 0.10