BÖHLER A959

BÖHLER A959 (Alloy 28, UNS N08028, W. Nr. 1.4563) is a nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as pitting and crevice corrosion. The alloy is especially resistant to sulphuric and phosphoric acid. Equipment used for chemical processing, pollution control equipment, oil and gas well piping ,natural gas and oil transportation, nuclear fuel reprocessing and transportation, acid production and pickling equipment and transportation
The alloy was originally developed for use in the manufacture of phosphoric acid, especially for heat exchangers in the concentration unit, where corrosive conditions are at their worst.

Forme di prodotto disponibili

Prodotti lunghi: I dati presentati si riferiscono esclusivamente ai prodotti lunghi. Si prega di osservare le spiegazioni dettagliate alla fine della scheda tecnica (pdf).

Percorso di fusione

Forno ad arco/EAF

Numeri del materiale

Market grade
Alloy 28
SEL
1.4563
EN
X1NiCrMoCu31-27-4
UNS
N08028

Standard

EN ISO
10088-3

Composizione chimica

* Composizione chimica (media %)

C
max. 0.020
Si
max. 0.70
Mn
max. 2.00
P
max. 0.030
S
max. 0.010
Cr
26.0 to 28.0
Mo
3.0 to 4.0
Ni
30.0 to 32.0
Cu
0.70 to 1.50
N
max. 0.10

Applicazioni